← Hume Pipes

Three Edge Bearing Test (Hume Pipes)

Format · 0.25 mm crack load · IS:458-2003 & IS:3597-1998

Fill in the specimen and ram details, or leave the sheet empty to print a blank format. Area of rams = n × πd²/4, load to be applied = 0.25 mm crack load requirement (kN/m) × length of pipe (m), and the matching gauge pressure (kg/cm²) are worked out as you type. Typed values are saved for this project.

THREE EDGE BEARING TEST (0.25mm Crack Load)
(As per IS:458 -2003 And IS :3597-1998)
Lot No:
Date of Testing:
Specimen No.:
Dia of Ram (d) (mm):
No of jacks (n):
Area of Rams (n × πd²/4):
Length of Pipe (m):
0.25 mm crack load requirement as per IS 458 - 2003 (kN/m):
Hence, load to be applied for 0.25mm Crack is
S.No.Pipe Ref. NoApplied Load (kg/Sqcm)
1
2
Remarks :
Name:
Date:
Contractor's Representative
Name:
Date:
Concessionaire's/PMC Representative
Name:
Date:
IE's Representative